Specification
State |
Powdered |
Application |
Boiler work and power plant, the cold crushing |
Cold crushing strength |
350 to 450 Kg / cm |
Features:
Product |
Al2O3 |
Fe2O3 |
B. D. |
Cold Crushing Strength |
PLC |
PCE |
Grain Size |
||
% |
% |
% |
Kg / cm2 |
% |
Degree C |
mm |
|||
Min. |
Max. |
Min. |
Dried at 110 degree C/24 hrs Min. |
Fired at 1400 degree C/3 hrs Min. |
Fired at 1500 degree C/3 hrs Min. |
Max. |
Min. |
|
|
TRL Cast FH 14 |
40 |
2.5 |
1.90 |
250 |
350 |
- |
-/+ 1.5 (1400 degree C / 3h) |
1580 |
0-5 |
TRL Cast FH 45 |
45 |
4 |
2.10 |
250 |
350 |
- |
-/+ 1.5 (1400 degree C / 3h) |
1580 |
0-5 |
TRL Cast FH 70 |
70 |
5 |
2.40 |
350 |
450 |
- |
-/+ 1.5 (1400 degree C / 3h) |
1680 |
0-5 |